Please Log In



Forgot your password?

Hop on board...

Are you a new Customer? Click here to register.

Register
Loading Zoom, please wait
Sloped Square Plate Mould 8418 (17.8 x 17.7 x 2cm)Sloped Square Plate Mould 8419 (21.8 x 21.7 x 2.6cm)

Sloped Square Plate Mould 8418 (17.8 x 17.7 x 2cm)

Price £29.82 Inc VAT (£24.85 ex VAT)

 Go Back to Square Moulds 

All prices include VAT.

Ref: HU84805000 Stock Status: 10 Units in Stock
Ref:
P034
We Also Recommend for Sloped Square Plate Mould 8418 (17.8 x 17.7 x 2cm):
Product Information
Sloped Square Plate Mould

A simple and contemporary design perfect as a standalone dish or as part of a set. This easy shape is shallow with slightly upturned corners adding depth to your glass project.

Dimensions: 

Inner: Length: 16.6cm, Width: 16.5cm, Height: 1.6 cm

Outer: Length: 17.8 cm, Width: 17.7 cm, Height: 2 cm

Please note that all our moulds are hand-made and therefore the dimensions may vary slightly from those shown. Mould manufacturers allow a tolerance of up to 2cm. We strongly recommend cutting the glass to the size measured from the actual mould rather than relying solely on the dimensions shown.

Firing Schedule:

Please note: This firing recommendation has been calculated using Bullseye Glass with a thickness of 6 mm in a Paragon GL24 kiln, and is courtesy of Bullseye Glass Co. 

Segment Rate (C/hr) Temp. Hold
1 167C 638C :05
2 999 482C 1:00
3 56C 371C :00

Troubleshooting:

  • Small kilns may require the process temperature reducing. In the Hobbyfuser and HotStart Pro, reduce the top temperature from 649C to 626C. In the Firebox 14, reduce the top temperature from 649C to 606C. All kilns vary, as does glass viscosity. Testing is necessary.

  • Remove the shelf when slumping in small kilns.

  • Side firing kilns may require more time in the first ramp than top firing kilns.

  • Bubbles in slumping are caused by firing too high or holding too long at process temperature.

  • Cracked moulds or cracked glass is caused by firing too fast in the first ramp or cooling too fast.

  • Devitrification on the outside of a slumped piece is caused by firing too high or holding too long at process temperature.

All our moulds are designed for multiple use and with care should last for many firings.

Use with mould 8417 and 8419 to create a stunning tableware set, great for your home or as a gift!


Product Reviews

There are currently no reviews for this product. Be the first to Write a review

Registered office: 5 Havyat Park, Wrington, Bristol, BS40 5PA, UK
Company Reg No. 5365166. VAT No. 791350132
© Warm Glass UK, 2015-2018
Registered office: 5 Havyat Park, Wrington, Bristol, BS40 5PA, UK
Company Reg No. 5365166. VAT No. 791350132